The electrical resistivity, Hall coefficient and thermoelectric power have been measured over the temperature range from 4.2 to 800°K on Co 1- x Mn x Si(\(x{\lesssim}0.06\)), Co 1- x Cr x Si(\(x{\lesssim}0.04\)) and, Co 1- x Cr x Si(\(x{\lesssim}0.10\)) solid solutions. The specimen is n -type when ...