The electrical resistivities, Hall coefficients and thermoelectric powers of undoped, Si-doped and Mn-modified CrSi 2 crystals have been measured over the temperature range from 90°K to 1100°K. The undoped crystal is a p -type semiconductor with the hole concentration of about 4×10 20 /cm 3 . The ho...