We synthesized nano-ZnCo 2 O 4 using molten salt method at low temperature 280°C for 30 min or 3h in air, at a heating and cooling rate of 3°C/min and quenching. Reported are the effects of Co-sulphate, hydroxide and Zn-sulphate salt combinations, and heating, cooling rate on morphology and crystal ...