Oak has been converted to a porous biocarbon template by annealing in an inert atmosphere above 800°C. Subsequent infiltration with gaseous SiO at 1550–1600°C under flowing argon of atmospheric pressure finally resulted in the formation of a porous, cellular β‐SiC ceramic. The conversion retains the...