Synchrotron X-rays on the Swiss Norwegian Beamline and BM28 (XMaS) at the ESRF have been used to record the diffraction response of the PMN–PT relaxor piezoelectric 67% Pb(Mg1/3Nb2/3)O3–33% PbTiO3as a function of externally applied electric field. A DC field in the range 0–18 kV cm−1was applied alon...